. 2021 Sep 8;14(18):5160. doi: 10.3390/ma14185160

Table 3.

Results of control chemical analysis of bar forged from heat A [wt.%].

Sampling Location C Mn Si P S Cu Ni Cr Mo Al Ce N O
Subsurface 0.435 0.67 0.257 0.0060 0.0050 0.138 0.199 1.02 0.147 0.024 0.023 0.00622 0.00348
¼ of diameter 0.446 0.67 0.259 0.0060 0.0056 0.141 0.201 1.03 0.148 0.023 0.027 0.00589 0.00113
Center 0.454 0.69 0.285 0.0063 0.0057 0.135 0.127 1.03 0.157 0.025 0.028 0.00743 0.00181