Table 1.
Sample | Elongation at Break (%) | Tensile Strength (MPa) | Tensile Modulus (MPa) |
---|---|---|---|
PU | 91 ± 3.5 | 0.75 ± 0.08 | 0.95 ± 0.15 |
PU-NL | 96 ± 5.6 | 0.91 ± 0.1 | 1.25 ± 0.45 |
PU-NL/EEP | 73 ± 3.9 | 0.82 ± 0.09 | 0.84 ± 0.19 |
Sample | Elongation at Break (%) | Tensile Strength (MPa) | Tensile Modulus (MPa) |
---|---|---|---|
PU | 91 ± 3.5 | 0.75 ± 0.08 | 0.95 ± 0.15 |
PU-NL | 96 ± 5.6 | 0.91 ± 0.1 | 1.25 ± 0.45 |
PU-NL/EEP | 73 ± 3.9 | 0.82 ± 0.09 | 0.84 ± 0.19 |