. 2021 Sep 28;430:132723. doi: 10.1016/j.cej.2021.132723

Fig. 4.

Fig. 4

a) and b) Cycling performance of Li//Li symmetric cell with blank PP and S-MF, respectively, at a current density at 0.5 mA cm−2 (for 0.5 mAh cm−2); c) detailed voltage profiles from Fig. 4a and b; d) LSV curves of Li//separator//SS cells at scan rate of 0.1 mV s−1; e) Nyquist plots of Li//separator//SS cells.