Table 2. Nitrogen Adsorption–Desportion (BET) Data and Rietveld Refinement Obtained from SXRD and PND Data for the LMNO–Ar and LMNO–H2 Samples Obtained at 700 °C.
| Parameters | LMNO–Ar | LMNO–H2 | % difference |
|---|---|---|---|
| surface area (m2 g–1)a | 7.0 | 7.9 | 12.9 |
| pore volume (cm3g–1)a | 0.108 | 0.132 | 22.2 |
| pore size (nm)a | 60.1 | 67.0 | 11.5 |
| phase P4332 content (%)b | 86.2 | 94.1 | |
| phase Fd3̅m content (%)b | 0.10 | 5.9 | |
| rock salt (Li0.8Mn0.81O2) content (%)b | 13.7 | ||
| NiO impurity (%)c | 11.8 | 0.1 |
Nitrogen adsorption–desoprtion (BET) data.
SXRD Reitveld refinement.
PND Reitveld refinement.