. 2021 Sep 23;14(19):5501. doi: 10.3390/ma14195501

Figure 6.

Figure 6

SEM images of surfaces of fractured samples sintered at 1600 °C for 2 h; (a) only the mullite phase in the halloysite–boehmite mixture and (b) the presence of both mullite and zirconia (see arrows) in halloysite–boehmite–zirconia mixtures [50].