Skip to main content
. 2021 Sep 24;14(19):5531. doi: 10.3390/ma14195531

Figure 13.

Figure 13

Worn surface of an NAO pad: (a) SEM backscattered electron image; (bd) EDS spectra corresponding, respectively, to the areas labeled as b, c, and d in (a) (accelerating voltage 20 kV, working distance 15.3 mm).