Table 1.
Samples | Microhardness (HV) | Adhesion Strength (Mpa) |
---|---|---|
Uncoated Mg | 37.1 ± 1.5 | – |
AN-Mg | 58.5 ± 1.5 | 18.2 ± 0.4 |
DCPD-Mg | 66.4 ± 2.2 | 21.6 ± 0.3 |
HA-Mg | 88.8 ± 2.7 | 23.3 ± 0.5 |
Uncoated WE43 | 76.7 ± 2.5 | – |
AN-WE43 | 106.3 ± 3.5 | 19.6 ± 0.3 |
DCPD-WE43 | 120.0 ± 3.3 | 23.2 ± 0.2 |