Table 2.
Experiment | Fiber Mix-Proportion | HFRC (Kevlar 12 mm/ Carbon 24 mm) |
HFRC (Carbon 12 mm/ Kevlar 24 mm) |
Benchmark | Total |
---|---|---|---|---|---|
Compressive Test | 100–0% | 3 | 3 | 3 | 45 |
80–20% | 3 | 3 | |||
60–40% | 3 | 3 | |||
50–50% | 3 | 3 | |||
40–60% | 3 | 3 | |||
20–80% | 3 | 3 | |||
0–100% | 3 | 3 | |||
Flexural Test | 100–0% | 3 | 3 | 3 | 45 |
80–20% | 3 | 3 | |||
60–40% | 3 | 3 | |||
50–50% | 3 | 3 | |||
40–60% | 3 | 3 | |||
20–80% | 3 | 3 | |||
0–100% | 3 | 3 | |||
Splitting Tensile Test |
50–50% | 3 | 3 | 3 | 9 |
Impact Test | 50–50% | 20 | 20 | 20 | 60 |