Table 8.

Splitting tensile strengths of benchmark and HFRC specimens.

Specimen Benchmark HFRC Specimen (L12 mm/L24 mm)
S-B S-K5/C5 S-C5/K5
Splitting Tensile Strength (MPa) 2.33 3.09 2.96
2.46 3.16 2.99
2.48 3.21 2.99
Average Splitting Tensile Strength (MPa) 2.42 3.15 2.98
Increase (%) - 30 23