Skip to main content
. 2021 Sep 26;13(19):3290. doi: 10.3390/polym13193290

Figure 1.

Figure 1

AFM topographic image of m-GO film (a) before and (be) after conjugation with peptide at 2.5 µm × 2.5 µm and corresponding surface roughness measurements (f).