Skip to main content
. 2021 Sep 30;13(19):3368. doi: 10.3390/polym13193368

Figure 14.

Figure 14

SEM image from fractured surface (a) 0°, (b) 45°, (c) 90° and (d) +45°/−45°. Reprinted with permission from Ref. [48]. 2011, IntechOpen.