Skip to main content
. 2021 Oct 19;11:20665. doi: 10.1038/s41598-021-00181-1

Figure 7.

Figure 7

Temperature of the samples of polyurethane coating with 0, 1, 3, and 5% of nano ZrO2 and Al2O3.