  texture characteristics
 
sample SBET (m2/g) Vpore (cm3/g) Dpore (Å) the actual content of molybdenum (wt %)
10%Mo/Et3N-SBA-15 before oxidation 307 0.37 49 9.5
10%Mo/Et3N-SBA-15 after oxidation 301 0.36 48 9.5
10%Mo/H3N-SBA-15 before oxidation 319 0.38 52 9.7
10%Mo/H3N-SBA-15 after oxidation 310 0.36 51 9.6