Skip to main content
. 2021 Oct 5;6(41):26880–26887. doi: 10.1021/acsomega.1c03142

Figure 9.

Figure 9

XRD pattern of the Fe3O4/FTO electrodes at different polarization times (10 min and 5 h) at −1.3 V vs Ag/AgCl.