Skip to main content
. 2021 Oct 21;11:20777. doi: 10.1038/s41598-021-00148-2

Figure 5.

Figure 5

STEM bright field (BF) and annular dark field (ADF) images, EDX maps and SAED patterns from the EMD electrodes at different stages during cycling. (a) Electrode discharged at 1.35 V during the conditioning cycle, (b) electrode charged at 1.8 V during the 5th cycle, and (c) fully charged electrode held for 2 h at 1.8 V during the 50th cycle.