Figure 6.

Figure 6

SEM SE images of EMD electrodes at different potentials during cycling tests. (a) Conditioning cycle at 0.5 mA cm–2 and (b) the 5th cycle at 1 mA cm–2. EDX maps for the D0.9 V images. Discharge and charge processes are denoted as D and C, respectively.