Skip to main content
. 2021 Oct 19;14(20):6201. doi: 10.3390/ma14206201

Figure 13.

Figure 13

SEM micrographs of the fracture surface of PA12-ZrO2 at magnifications of ×30 (a), ×1000 (b), and ×2000 (c); PA12-Al2O3 at magnifications of ×30 (d), ×1000 (e), and ×2000 (f).