Table 5.
Area roughness of composite films deposited on glass slide substrates.
Film on Glass Slide Sample | Root Mean Square Height (µm) |
---|---|
Glass/5 layers NaPAC16 + MgO NPs (0.5%) | 0.02125 |
Glass/5 layers NaPAC16 + TiO2 NPs (0.5%) | 0.01107 |
Area roughness of composite films deposited on glass slide substrates.
Film on Glass Slide Sample | Root Mean Square Height (µm) |
---|---|
Glass/5 layers NaPAC16 + MgO NPs (0.5%) | 0.02125 |
Glass/5 layers NaPAC16 + TiO2 NPs (0.5%) | 0.01107 |