Table 6.
Sample | Glass | Glass/5 Layers NaPAC16 |
Glass/5 Layers NaPAC16 + MgO |
Glass/5 Layers NaPAC16 + TiO2 |
---|---|---|---|---|
Contact angle θ (°) | 41.26 | 74.50 | 98.79 | 78.50 |
Sample | Glass | Glass/5 Layers NaPAC16 |
Glass/5 Layers NaPAC16 + MgO |
Glass/5 Layers NaPAC16 + TiO2 |
---|---|---|---|---|
Contact angle θ (°) | 41.26 | 74.50 | 98.79 | 78.50 |