Maximum vertical substance loss (in mm) on the FDP surface (two samples) after chewing simulation in combination with thermocycling.

Directly Processed Indirectly Processed/ Indirectly Processed/
Temporary Temporary Permanent
FDPs S3 LC SC CT GD LE
1 1.52 0.42 0.81 0.87 0.85 0.05
2 - 1 0.56 0.55 0.81 0.78 0.07

1 The second test specimen failed during ageing.