(A) SEM micrograph of the bare electrode illustrates the surface is least heterogeneous with an average surface roughness of 0.03 µm. (B) DPV of the bare gold electrode in 0.1 M phosphate buffer, pH 7.0 (black curve) with DTT adsorbed on the gold surface (red curve).