Skip to main content
. 2021 Oct 11;9:705475. doi: 10.3389/fchem.2021.705475

FIGURE 6.

FIGURE 6

Compressive Strength development in alkali-activated synthetic glass (20 h, 85°C, 8M NaOH) with: (A) different SiO2/Al2O3 ratios; (B) the same ratio and different CaO contents (Legend: N represents glasses activated with NaOH, and V is the nomenclature for synthetic glass prepared with different S/A ratios).