Skip to main content
. 2021 Sep 1;55(3):116–123. doi: 10.26650/eor.2021872015

Table 1.

Flexural strength values of the groups (MPa). (SD: Standard deviation, H: Heat-polymerized polymethyl methacrylate, P: Polyamide, R: Glass fiber reinforced polyamide. aOne way ANOVA Test*p<0.001, bTukey Test **p<0.05, cPaired t Test***p<0.05).

Before Aging After Aging
Group Mean ±SD Mean ±SD cp
H 119.85 ±15.65 118.9 ±31.05 0.949***
P 80.13 ±12.74 75.3 ±15.53 0.554***
R 72.16 ±13.12 71.73 ±14.8 0.922***
ap 0.000* 0.000*
Pairwise H-P 39.72** H-P 43.6**
Comparisons; bp H-R 47.69** H-R 47.17**
P-R 7.97 P-R 3.56