Skip to main content
. 2021 Sep 1;55(3):116–123. doi: 10.26650/eor.2021872015

Table 5.

The glass transition temperatures of denture base materials before and after thermocycling procedure. (H: Heat-polymerized polymethyl methacrylate, P: Polyamide, R: Glass fiber reinforced polyamide).

Group Before aging After aging
H 144.53°C 138.40°C
P 134.26°C 132.26°C
R 134.22°C 130.79°C