Table 1.
Non-templated films | Urea-templated films | |
---|---|---|
Young’s Modulus (MPa) | 3.9 ± 1.1 | 3.3 ± 1.0 |
Tensile Strength (MPa) | 3.8 ± 1.0 | 4.6 ± 0.6 |
Elongation (%) | 97 ± 14 | 136 ± 22 |
Toughness (mJ) | 9.7 ± 2.9 | 36.4 ± 14.1 |
Storage Modulus (MPa) | 35.0 ± 4.7 | 22.1 ± 4.0 |
Loss Modulus (MPa) | 4.2 ± 1.1 | 2.7 ± 1.5 |
Gelation point (Hz) | 100 ± 3 | N/A |
Gelation point (Hz): Perpendicular to pores. | N/A | 77 ± 3 |
Gelation point (Hz): Parallel to pores. | N/A | 63 ± 4 |
% Elongation to break | 67 ± 4 | 93 ± 10 |