Skip to main content
. 2021 Oct 14;13(42):49692–49704. doi: 10.1021/acsami.1c13972

Table 1. Summary of the Main Preparation Characteristics of Hydrogels Prepared for the Present Work.

sample peptidesaused for the matrix addition of MNPb application of magnetic fieldc
FF Fmoc-FF no no
FF + MNP Fmoc-FF yes no
FF + MNP + H Fmoc-FF yes yes
FF + RGD Fmoc-FF + Fmoc-RGDd no no
FF + RGD + MNP Fmoc-FF + Fmoc-RGDd yes no
FF + RGD + MNP + H Fmoc-FF + Fmoc-RGDd yes yes
a

Peptide concentration was 20 mM in all cases.

b

Concentration of MNP was 0.1 vol %. MNP were previously double-coated with PEG + Fmoc-FF.

c

Strength of the magnetic field was H = 15 kA m–1 and was maintained during the first hour of gelation.

d

The Fmoc-FF-to-Fmoc-RGD ratio was 7:3.