Skip to main content
. 2021 Oct 21;60(21):16713–16725. doi: 10.1021/acs.inorgchem.1c02582

Figure 12.

Figure 12

(A) Nyquist plot for 35– using a Pt electrode. (B) Bode plot using a Pt electrode. (C) Nyquist plot for 35– using a GC electrode. (D) Bode plot using a GC electrode. The working potentials for each curve were −0.520 V (black circles), −0.890 V (red circles), −1.220 V (green circles), −1.560 V (blue circles), and −1.910 V (purple circles).