. 2021 Oct 20;13(43):51767–51774. doi: 10.1021/acsami.1c15607

Figure 4.

Figure 4

Stripping–plating behavior of symmetric Li/Na cells after initial cell assembly vs after 600 h of storage (applied current: 0.1 mA cm–2) with (a,b) triglyme and (c,d) carbonate electrolytes. Top-view images of the electrode after stripping–plating measured by SEM are shown in Figure S11.