Skip to main content
. 2021 Nov 1;31:41–51. doi: 10.1016/j.jot.2021.10.002

Figure 3.

Figure 3

A. Weight of scaffolds after degradation; B. pH value in the degradation medium; C.The released ratio of CuB in degradation medium; D. The rest ratio of CuB in residual PT/CuB scaffold; E. The accumulated content of CuB in PT/CuB scaffold degradation medium and the residual PT/CuB scaffold; F. The tube formation of EA.hy926 ​cells which were treated by CuB from PT/CuB scaffold degradation medium. G. AR staining images which hBMSCs were treated by CuB from PT/CuB scaffold degradation medium; H & I. The effects on total master segments length and total meshes area treated by CuB from PT/CuB scaffold degradation medium (∗p ​< ​0.05, ∗∗p ​< ​0.01, n ​= ​5); J. Quantitative analysis of mineralization formation (∗p ​< ​0.05, ∗∗p ​< ​0.01, n ​= ​3).