TABLE 4.
Various Pt-based metal catalysts used for hydrogen production via APR method.
| Metal | Support | Hydrogen yield | Conversion (%) | References |
| Pt | CMK-3 | 57.5% | 79.4 | Kim et al. (2012a) |
| Pt | CMK-9 | 94.2% | 89.2 | Kim et al. (2012a) |
| Pt | CMK-3-MCN-R | 71.7% | 84.7 | Jeong et al. (2014) |
| Pt | CMK-5-MCN-R | 8.6% | 88 | Jeong et al. (2014) |
| Pt-Re | CMK-3 | 19.9 cm3/(gcat·min) | 44.2 | Kim et al. (2012b) |
| Pt-Ni | γ-Al2O3 | — | 80 | De Vlieger et al. (2012) |
| Pt-Fe | γ-Al2O3 | 48.1 cm3/(gcat·min) | 48.1 | Huber et al. (2006) |
| Pt-Re | CMK-3 | 36.6 cm3/(gcat·min) | 89.3 | Kim et al. (2012b) |