Rheological parameters calculated for placebo and SBE/Cs 80:500 loaded hydrogels.

P1 P2 F1-2 F1-4 F2-2 F2-4
Controlled rate
K 188.53 ± 5.42 9.07 ± 0.64 186.67 ± 4.00 113.17 ± 7.06 --- ---
n 0.11 ± 0.00 0.74 ± 0.02 0.10 ± 0.00 0.11 ± 0.00 --- ---
τ0 --- 316.53 ± 8.46 --- --- --- ---
Temperature sweeping
Tsol–gel 26.65 ± 0.11 25.68 ± 0.02 26.75 ± 0.04 26.28 ± 0.03 26.62 ± 0.02 25.80 ± 0.02
ηsol–gel 8.45 ± 0.07 13.02 ± 0.47 12.21 ± 0.04 9.62 ± 0.03 10.61 ± 0.05 16.93 ± 0.03
Stress sweeping
LVR 74.83 ± 9.05 106.34 ± 10.01 84.48 ± 20.90 66.31 ± 18.08 62.07 ± 10.13 70.63 ± 13.13
Cross-over ↑ 158.43 ± 1.40 189.87 ± 5.09 165.97 ± 13.90 147.82 ± 20.64 168.77 ± 11.12 195.77 ± 10.37
Cross-over ↓ 92.88 ± 3.13 122.67 ± 12.19 92.73 ± 0.35 89.10 ± 5.15 87.73 ± 4.10 122.10 ± 7.24

K—consistency coefficient, n—power law index, τ0—yield point, Tsol–gel—gelation temperature, ηsol–gel—dynamic viscosity at Tsol–gel, LVR—linear viscoelastic region, Cross-over ↑—G′ = G″ point at increasing stress ramp, Cross-over ↓—G′ = G″ point at decreasing stress ramp.