Skip to main content
. 2021 Oct 27;14(21):6434. doi: 10.3390/ma14216434

Figure 3.

Figure 3

Figure 3

Temperature-dependent XRD patterns for Li(Fe1xMnx)0.88V0.08PO4 samples upon heating to 580 °C in nitrogen flow. Reference patterns for LiFePO4 (LFP), LiMnPO4 (LMP), and Li3V2(PO4)3 (LVP) are given below. Figure (b) reproduced from Ref. [12] by permission of IOP Publishing. © The Electrochemical Society. All rights reserved.