Skip to main content
. 2021 Oct 27;14(21):6446. doi: 10.3390/ma14216446

Figure 17.

Figure 17

Axial depth of cut ap versus surface roughness parameter RSm in the milling process performed using a tool coated with: (a) TiB2 and (b) TiAlN; (vc = 800 m/min; fz = 5 µm/tooth).