Skip to main content
. 2021 Aug 31;27(57):14307–14316. doi: 10.1002/chem.202102481

Figure 3.

Figure 3

Selected SEM micrographs for self‐assembled hybrid PNA‐peptide systems drop‐cast from a 20 mg ⋅ mL−1 solution: H−gcFF−OH (A), H−gcFF−NH2 (B). H−FFgc−NH2 (C) and H−FFgc−OH (D). Magnification and scale bar for all the samples correspond to 2450× and 30 μm.