Skip to main content
. 2021 Nov 9;14(22):6751. doi: 10.3390/ma14226751

Figure 6.

Figure 6

Comparission of microstructure (×1000) after heating at different temperatures ((A) 23 °C); ((B) 105 °C); ((C) 200 °C); ((D) 400 °C); ((E) 800 °C); ((F) 800 °C).