Skip to main content
. 2021 Nov 18;13(22):3989. doi: 10.3390/polym13223989

Figure 2.

Figure 2

X-ray diffraction patterns obtained after the annealing of the composites at 900 °C. 1—sample; 2—sample 2; 3—sample 3. All peaks correspond to HA (card #9-432) (samples 1–3, Table 1).