Skip to main content
. 2021 Nov 14;13(22):3932. doi: 10.3390/polym13223932

Figure 8.

Figure 8

The load-displacement curves of 3 mol% Y2O3-ZrO2 nanofiber mat and undoped zirconia nanofiber mat prepared at 900 °C.