. 2021 Nov 14;13(22):3932. doi: 10.3390/polym13223932

Table 1.

The specific surface area and pore volume of 3 mol% Y2O3-ZrO2 nanofibers calcined at different temperatures.

Calcination Temperature, °C Specific Surface Area, m2/g Pore Volume, cm3/g
700 23.6 0.051
900 15.1 0.037
1100 9.3 0.022