. 2021 Sep 23;10:222–235. doi: 10.1016/j.bioactmat.2021.09.003

Fig. 2.

Fig. 2

SEM images of unpolished cylinders after 3 h of sintering at 1100 °C of 4 selected Ca/P molar ratios: (a) 1.442; (b) 1.478; (c) 1.500 and (d) 1.552. These cylinders were all made out of β-TCP powders calcined at 850 °C for 1 h. The scale bar is 2 μm for all 4 images.