TABLE 1.
Geometrical, material, and operating conditions used in current spheroid-on-a-chip design study.
Parameter | Notation | Range | Steps | Number of conditions | References |
---|---|---|---|---|---|
Inlet velocity left | Q1 | 0.01–0.02 ml/h | 0.01, 0.02 ml/h | 2 | Patra et al. (2016); Moshksayan et al. (2018) |
Inlet velocity right | Q2 | 0.01–0.02 ml/h | 0.01, 0.02 ml/h | 2 | Patra et al. (2016); Moshksayan et al. (2018) |
Infusion width left | WL | ∼0–60 µm | 0.1, 20, 30, 40, 60 µm | 5 | Cohen et al. (2010); Ota et al. (2010); McMillan et al. (2016) |
Infusion width right | WR | 20–60 µm | 20, 30, 40, 60 µm | 4 | Cohen et al. (2010); Ota et al. (2010); McMillan et al. (2016) |
Infusion height left | HL | ∼0–60 µm | 0.1, 20, 30, 40, 60 µm | 5 | Cohen et al. (2010) |
Infusion height right | HR | 20–60 µm | 20, 30, 40, 60 µm | 4 | Cohen et al. (2010) |
Chamber radius | R | 80–160 µm | 80, 120, 160 µm | 3 | Cohen et al. (2010) |
Porosity | 0.2–0.9 | 0.2, 0.5, 0.7, 0.9 | 4 | Hwang et al. (2010) |