Skip to main content
. 2021 Nov 27;14(23):7260. doi: 10.3390/ma14237260

Figure 1.

Figure 1

SEM and surface topography micrographs of (a) as-built L-PBF Ti6Al4V(ELI), (b) Ti6Al4V(ELI)-3 at.% Cu surfaces, and (c) after grinding process (same surface topography was obtained for both samples with and without 3 at.% Cu).