Skip to main content
. 2021 Nov 24;14(23):7155. doi: 10.3390/ma14237155

Figure 10.

Figure 10

(a) TEM bright field images showing precipitates in the α-Al matrix. (b,d) The corresponding selected area diffraction patterns obtained from the samples aged at 480 °C for 1h, together with (c) the simulated diffraction pattern of α-Al15 (Fe, Mn)3Si2 phase.