Skip to main content
. 2018 May 1;12(6):807–813. doi: 10.1049/iet-nbt.2018.0044

Fig. 9.

Fig. 9

XRD spectra of pure cellulose powder and the corresponding electrosprayed nanoparticles [concentration = 2% (w/w), voltage = 23 kV, nozzle–collector distance = 10 cm and feed rate = 0.03 ml/h]

(a) Molecular weight = 120 KDa, (b) Molecular weight = 192 KDa