Skip to main content
. 2021 Jan 13;11(5):2854–2865. doi: 10.1039/d0ra09182k

Raman spectroscopy data. Peaks position ( Created by potrace 1.16, written by Peter Selinger 2001-2019 D, Created by potrace 1.16, written by Peter Selinger 2001-2019 G), graphite peak (G), defect disorder peak (D), the degree of graphitization using the ratio of the integrated area intensity of graphite, and the intensity area of defect disorder peak (ID/IG). Sheet resistance (R) and conductivity (σ) of the activated films on the glass substrates.

Samples Created by potrace 1.16, written by Peter Selinger 2001-2019 D (cm−1) Area ID Created by potrace 1.16, written by Peter Selinger 2001-2019 G (cm−1) Area IG I D/IG R (kΩ sq−1) σ a (S m−1)
AC1 1347 147 1586 86 1.7 2.9 ± 0.3 13.9 ± 1.5
AC2 1346 88 1588 56 1.6 49.2 ± 13 0.86 ± 0.3
AC3 1341 92 1587 47 1.9 52.4 ± 7.9 0.75 ± 0.1
AC4 1344 114 1592 31 3.6 43.3 ± 11 0.94 ± 0.2
AC5 1339 120 1593 31 3.8 241.9 ± 76 0.12 ± 0.04
a

Conductivity measured via the 4-point probe method on the film containing the PVP binder.