Skip to main content
. 2021 Jan 21;11(7):3952–3962. doi: 10.1039/d0ra07529a

Fig. 4. XRD spectra for Ni nanowires in PAAM: (A) – HPAAM = 70 μm, j = 1.5 mA cm−2, t = 120 min (sample 1); (B) – HPAAM = 75 μm, j = 2 mA cm−2, t = 240 min (sample 2); (C) – HPAAM = 55 μm, j = 3 mA cm−2, t = 240 min (sample 3); (D) – HPAAM = 55 μm, j = 4 mA cm−2, t = 240 min (sample 4).

Fig. 4