The maximum temperature (Tmax) of AuNR/R-SiO2 after exposed to 808 nm laser at 2.0 W cm−2 for 8 min and their corresponding LSPR after heated at different temperature for 1 h.

Temperature (°C) LSPR (nm) T max (°C)
Control 935.0 60.5
400 859.0 75.8
500 850.5 81.1
600 839.0 84.8
700 829.0 89.5