Figure 2.

Room-temperature θ–2θ scans measured in the (00l) direction for GCMO thin films grown on (a) STO, (b) SLAO, (c) LSAT, and (d) MGO substrates. The intensity is given in the logarithmic scale. The peak marked with an asterisk (*) is an unidentified peak or arises from the sample holder. The inset shows the detail of the (004) peak together with the bare substrate.