. 2021 Apr 22;11(25):15118–15130. doi: 10.1039/d1ra02192c

The pore structure parameters of activated charcoal monoliths.

Conditions (°C–h) ρ (g cm−3) S BET (m2 g−1) V (cm3 g−1) P (%) d (nm)
300–0 0.182 ± 0.005 226 0.12 68 2.15
300–0.5 0.180 ± 0.001 493 0.20 84 1.63
300–1 0.175 ± 0.003 567 0.23 86 1.61
300–2 0.180 ± 0.004 565 0.23 85 1.61
300–3 0.183 ± 0.004 617 0.25 84 1.63
350–1 0.171 ± 0.001 601 0.25 84 1.67
400–1 0.169 ± 0.002 469 0.22 64 1.84