Skip to main content
. 2021 Dec 8;7(4):254. doi: 10.3390/gels7040254

Table 3.

Time (hours) necessary to release 25, 50, 75, 80, and 90% of IBU loaded in nanoconjugate hydrogels S3 and S6.

Kinetic Parameters S3 S6
T25% 0.249 0.061
T50% 2.179 0.948
T75% 7.740 4.719
T80% 9.470 6.093
T90% 13.686 9.712