Skip to main content
. 2021 Dec 11;7(4):257. doi: 10.3390/gels7040257

Figure 1.

Figure 1

Effect of drying time, water temperature, and CMC thickness on moisture content (PP 0.83, PP 0.55, PP 0.38, Inline graphic LDPE 0.15, Inline graphic LDPE 0.10, Inline graphic LDPE 0.03, Inline graphic PET 0.25, Inline graphic PET 0.18, Inline graphic PET 0.08).